GE OEC Medical Systems, Inc GE 4 inch Anterior Cervical Post, GE Part Number 1006385 or 1006385-NAV, GE Healthcare OEC Medical Systems (an accessory used with the InstaTrak 3500 plus and 9800 C-Arm Navigation systems) Recall
Check Your Product
According to the U.S. Food and Drug Administration (FDA)
Product
GE 4 inch Anterior Cervical Post, GE Part Number 1006385 or 1006385-NAV, GE Healthcare OEC Medical Systems (an accessory used with the InstaTrak 3500 plus and 9800 C-Arm Navigation systems)
Brand
GE OEC Medical Systems, Inc
Lot Codes / Batch Numbers
ALL LOT NUMBERS -GE Part number 1006385 or 1006385-NAV
Products Sold
ALL LOT NUMBERS -GE Part number 1006385 or 1006385-NAV
GE OEC Medical Systems, Inc is recalling GE 4 inch Anterior Cervical Post, GE Part Number 1006385 or 1006385-NAV, GE Healthcare OEC Medical S due to Weld defect- the weld between the post body and the screw was not properly formed and can fail, even when minimal force is used.. Based on FDA medical device recall database.
Summary derived from FDA notice
Reason for Recall
As stated by FDA
Weld defect- the weld between the post body and the screw was not properly formed and can fail, even when minimal force is used.
Recommended Action
Per FDA guidance
Consignees were notified by letter on 05/31/2006
Verify this information on the official source
For complete details and official instructions, check the U.S. Food and Drug Administration (FDA) directly.
View official FDA recall noticePage updated: Jan 10, 2026